The part in Problem 33.1 is to be fabricated using fused deposition modeling instead of\nstereolithography. Layer thickness is to be 0.20 mm and the wi
The part in Problem 33.1 is to be fabricated using fused deposition modeling instead of
\r\nstereolithography. Layer thickness is to be 0.20 mm and the width of the extrudate deposited on
\r\nthe surface of the part = 1.25 mm. The extruder workhead moves in the x-y plane at a speed of
\r\n150 mm/s. A delay of 10 s is experienced between each layer to reposition the workhead.
\r\nCompute an estimate for the time required to build the part.