A spot weld was made using an arc-welding process. In a spot-welding operation, two 1/16-in-thick\naluminum plates were joined. The melted metal formed
A spot weld was made using an arc-welding process. In a spot-welding operation, two 1/16-in-thick
\r\naluminum plates were joined. The melted metal formed a nugget that had a diameter of ¼ in. The
\r\noperation required the power to be on for 4 sec. Assume the final nugget had the same thickness as
\r\nthe two aluminum plates (1/8 in thick), the heat transfer factor was 0.80 and the melting factor was
\r\n0.50. Determine the rate of heat generation that was required at the source to accomplish this weld.